Datasheet summary
LEWATIT® A 8072 +
PDF datasheet mirror for LEWATIT® A 8072 + (Lanxess LEWATIT). Verify with OEM before design.
Summary
Product identification
Lewatit® A 8072+ is a heterodisperse, weakly basic anion exchange resin based on a gel-type acrylic-divinylbenzene matrix.
Common Description:
- Delivery form: free base
- Functional group: tertiary amine
- Matrix: acrylic
- Structure: gel
- Appearance: ivory, translucent
Operating limits
- Stability pH range: 0 - 14
- Operating temperature: max. 60 °C
- Max. pressure loss during operation: 150 kPa
Feed water
Lewatit® A 8072+ is suitable for demineralization of water for industrial steam generation, especially in systems with high organic fouling potential. It is also effective for removing organic matter, particularly from surface water.
Product water
This resin is particularly recommended for applications requiring low silica leakage, especially when combined with a strong dissociated anion exchange resin.
Electrical
No information available in the extract.
Mechanical / hydraulic
- Uniformity coefficient: max. 1.6
- Effective size (d10): 0.50 - 0.74 mm
- Fines (less than 0.315 mm): max. 1 vol %
- Total capacity (delivery form): min. 1.4 eq/L
- Bulk density for shipment (+/- 10%): 710 g/L
- Density: approx. 1.1 g/mL
- Water retention (delivery form): approx. 56-64 % weight
- Volume change (free base - Cl⁻): max. approx. 12 %
- Bed depth for single column: min. 800 mm
- Backwash bed expansion (per m/h at 20°C): 15 %
- Specific pressure loss (at 15°C): 1.1 kPa*h/m²
- Specific flow rate: max. 40 BV/h
Regeneration
- NaOH regeneration concentration: approx. 2-6 wt. %
- NaOH regeneration quantity (co-current): min. 80 g/L resin
- NaOH regeneration quantity (counter-current): min. 50 g/L resin
- Regeneration contact time: min. 30 minutes
- Slow rinse (at regeneration flow rate): min. 3 BV
- Fast rinse (at service flow rate): min. 5 BV
Additional Information
- Safety: Strong oxidants can cause violent reactions. Observe the safety data sheet.
- Disposal: Dispose according to European waste nomenclature.
- Storage: Store above freezing point, dry, under roof, out of direct sunlight. Thaw frozen resin gradually. Packaging stability is limited to 24 months under recommended storage conditions.
Disclaimer: This extraction may miss figures, footnotes, or revisions. Contractual data must match the OEM PDF revision used on the project.
Official datasheet (PDF)