Datasheet summary
LEWATIT® MonoPlus M 500 KR
PDF datasheet mirror for LEWATIT® MonoPlus M 500 KR (Lanxess LEWATIT). Verify with OEM before design.
Summary
Product identification
- Product Name: LEWATIT® MonoPlus M 500 KR
- Description: Strongly basic, premium grade, gel-type anion exchange resin (type I) with beads of uniform size (monodisperse) in highly regenerated and purified form to meet nuclear industry specifications.
- Functional group: Quaternary ammonium (OH⁻)
- Matrix: Styrenic
- Structure: Gel
- Appearance: Light brown, translucent
- Delivery form: OH⁻
Applications
LEWATIT® MonoPlus M 500 KR is particularly suitable for:
- Removal of anions, including radioactive isotopes, from aqueous solutions (including boric acid).
- Decontamination of circuits in nuclear reactor plants.
- Treatment of primary coolant e.g. in pressure water reactors.
- Purification of steam generator blow down irrespective of conditioning with Levoxin (hydrazine), ethanolamine or morpholine.
- Polishing in primary and secondary sections as a mixed bed component with Lewatit® MonoPlus SP 112 KR or Lewatit® MonoPlus S 200 KR.
Specified Data
- Uniformity coefficient: max. 1.1
- Mean bead size (d₅₀): 0.64 (+-0.05) mm
- Total capacity (delivery form): min. 1.1 eq/L
Typical Physical and Chemical Properties
- Bulk density for shipment (+/- 5%): 670 g/L
- Density: approx. 1.07 g/mL
- Water retention (delivery form): approx. 56-62 % weight
- Stability pH range: 0-14
- Storage temperature range: -20 - +40 °C
- Friability: >200 g/bead min. vol % (average 700 g/bead)
- Ionic conversion OH⁻: min. 95 eq. %
- Ionic conversion CO₃²⁻: max. 5 eq. %
- Ionic conversion Cl⁻: max. 0.5 eq. %
- Ionic conversion SO₄²⁻: max. 0.5 eq. %
Operation
- Operating temperature: max. 70 °C
- Operating pH range during exhaustion: 0-12
- Bed depth for single column: min. 800 mm
- Bed depth per component in mixed bed: min. 500 mm
- Backwash bed expansion (per m/h at 20°C): 11 %
- Specific pressure loss (at 15°C): 1 kPa*h/m²
- Max. pressure loss during operation: 250 kPa
- Specific flow rate: max. 100 BV/h
Trace Impurities (max. mg/kg dry resin)
- Na: 20
- Fe: 30
- Cu: 5
- Al: 5
- Co: 5
- Pb: 10
- Hg: 5
- SiO₂: 50
- Total Chloride: 500
- SO₄²⁻ as Sulphur: 600
Storage and Handling
- Storage Temperature: Recommended above freezing point of water, under roof, dry, and out of direct sunlight.
- Frozen Resin: Allow to thaw gradually at ambient temperature before handling or use; do not accelerate thawing.
- Packaging Stability: Limited to 24 months under recommended storage conditions. Use within this timeframe or check packaging condition regularly.
- Safety Precautions: Avoid contact with strong oxidants (e.g., nitric acid) which can cause violent reactions. Observe the safety data sheet for further information on transport, storage, handling, safety, and ecology.
Disposal
- Dispose of ion exchange resins according to the European waste nomenclature within the European Community.
Disclaimer: Extraction may miss figures, footnotes, or revisions; contractual data must match the OEM PDF revision used on the project.
Official datasheet (PDF)
Curated from selected public technical reference material for discovery and preliminary comparison. This summary is not a substitute for a current certified manufacturer datasheet. Verify revisions and design limits before use.