LEWATIT® MonoPlus TP 209 XL

PDF datasheet mirror for LEWATIT® MonoPlus TP 209 XL (Lanxess LEWATIT). Verify with OEM before design.

Summary

Product identification

LEWATIT® MonoPlus TP 209 XL is a weakly acidic, macroporous cation exchange resin with iminodiacetate (IDA) groups. It is designed for the selective extraction of heavy metal cations from weakly acidic to weakly basic solutions. This resin is particularly suited for concentration, extraction, and recovery of base metals in Resin-in-Pulp (RIP) processes due to its large bead size and high operational capacity.

The cation removal order is: Fe³⁺ > Cu²⁺ > VO₂²⁺ > UO₂²⁺ > Pb²⁺ > Ni²⁺ > Zn²⁺ > Cd²⁺ > Fe²⁺ > Mn²⁺ > Ca²⁺ > Mg²⁺ >> Na⁺.

Compared to LEWATIT® MonoPlus TP 207, LEWATIT® MonoPlus TP 209 XL offers:

  • Lower dynamic pressure drop at the same flow rate
  • Diminished risk of accumulation of suspended solids
  • Easier screening and sieving during resin/feed separation

Common Description:

  • Delivery form: Na⁺
  • Functional group: Iminodiacetic acid
  • Matrix: Styrenic
  • Structure: Macroporous
  • Appearance: White, opaque

Operating limits

  • Stability pH range: 0-14
  • Stability temperature range: 1-80 °C
  • Storage temperature range: -20 - +40 °C
  • Operating temperature: max. 80 °C
  • Operating pH range during exhaustion: 2-10

Mechanical / hydraulic

  • Uniformity coefficient: max. 1.1
  • Mean bead size: 0.85 (±0.05) mm
  • Total capacity (H⁺ form): min. 2.4 eq/L
  • Bulk density for shipment (±5%): approx. 709 g/L
  • Density: approx. 1.18 g/mL
  • Water retention (delivery form): approx. 50 % by weight
  • Volume change (H⁺ - Na⁺): max. approx. 35 %
  • Bed depth for single column: min. 1000 mm
  • Backwash bed expansion per m/h (20°C): 4 %
  • Specific pressure loss (15°C): 0.5 kPa*h/m²

Regeneration

  • HCl regeneration concentration: approx. 7 wt. %
  • H₂SO₄ regeneration concentration: approx. 10 wt. %
  • Regeneration contact time: min. 15 minutes

Conditioning

  • NaOH conditioning concentration: approx. 4 wt. %

Additional Information

  • Safety: Avoid contact with strong oxidants like nitric acid, which can cause violent reactions. Consult the safety data sheet for further details.
  • Disposal: Dispose of ion exchange resins according to European waste nomenclature regulations.
  • Storage: Store above freezing point, under roof, in dry conditions, and out of direct sunlight. If frozen, allow to thaw gradually at ambient temperature before handling or use.
  • Packaging: Packaging stability is limited to 24 months under recommended storage conditions. Regularly check packaging condition if used beyond this timeframe.

Disclaimer: Extraction may miss figures, footnotes, or revisions. Contractual data must match the OEM PDF revision used on the project.

Official datasheet (PDF)

Lenntech datasheet mirror

Curated from selected public technical reference material for discovery and preliminary comparison. This summary is not a substitute for a current certified manufacturer datasheet. Verify revisions and design limits before use.