Datasheet summary
SEPLITE MA900
PDF datasheet mirror for SEPLITE MA900 (SUNRESIN). Verify with OEM before design.
Summary
Product identification
- Product Name: SEPLITE® MA900
- Product Line: SEPLITE® Macro Strong Base Anion
- Stock Code: 300487
- Manufacturer Website: en.sunresin.com
Descriptions
SEPLITE® MA900 is a macroporous Type 1 strong base anion resin. Its unique structure facilitates the adsorption and desorption of organic and color substances, making it particularly effective for removing these from water and other solutions. It is also widely used in water treatment applications.
Physical and Chemical Characteristics
- Matrix Structure: Macroporous Polystyrene DVB
- Functional group: Quaternary Ammonium, Type 1
- Shipping form: OH⁻ form or Cl⁻ form
- Physical Appearance: Ivory spheres
- Particle size: 0.315-1.25 mm
- Moisture content: 50-60% (Cl⁻ Form)
- Total Capacity: ≥1.2 eq/L
- Bulk Density: 650-730 g/L
- Density: 1000-1100 g/L
- Whole beads count: ≥95%
Key features and benefits
- High operating capacity
- Good kinetic performance
- Long lifetime
Recommended Operating Conditions
- Maximum Operating Temperature: 35℃ (OH⁻ form), 70℃ (Cl⁻ form)
- Service Flow Rate: 5-50 BV/h
- Regeneration Temperature: ≤35℃
- Regenerant: NaOH
- Regenerant Concentration: 2-5%
- Regeneration Flow Rate: 3-10 BV/h
- Minimum Contact Time: 30 Minutes
- Fast Rinse Flow Rate: 4-7 BV/h
- pH Range: 0-14
1 BV (Bed Volume) = 1 m³ solution per m³ resin
Applications
- Industrial demineralization
- Radioactive element extraction
- Condensate deionization
- Removal of contaminants such as nitrate, arsenate, chromate, uranium etc.
Precautions
- Store resins in sealed containers or bags above 0℃ in dry conditions, away from direct sunlight.
- Avoid mixing ion exchange resin with strong oxidizing agents, as this can cause violent reactions.
- In case of eye contact, rinse immediately with plenty of water and consult a specialist.
- Dispose of material and samples according to local regulations.
- Dry polymers will expand when wetted and may cause an exothermic reaction.
- Spilled materials can be slippery.