Back to SUNRESIN
Sunresin logo

Datasheet summary

SEPLITE Monojet SC3200 Na

PDF datasheet mirror for SEPLITE Monojet SC3200 Na (SUNRESIN). Verify with OEM before design.

Summary

Product identification

SEPLITE® Monojet™ SC3200 Na is a gel, strong acid cation exchange resin with uniform particle size for industrial softening applications.

  • Stock Code: 300487
  • Matrix Structure: Gel, Styrene-divinylbenzene
  • Functional group: Sulfonic acid
  • Shipping form: Na⁺ (H⁺ is also available)
  • Physical Appearance: Dark brown translucent spherical beads

Physical and Chemical Characteristics

  • Particle size:
    • Nominal diameter: 0.65±0.05mm
    • Particles <0.3mm: ≤0.1%
    • Particles ≥0.85mm: ≤3.0%
  • Moisture content (Na⁺ Form): 39-45%
  • Total Capacity (Na⁺ Form): ≥2.2 eq/L
  • Bulk Density: 780-880 g/L
  • Density: 1250-1350 g/L
  • Whole beads count: ≥95%
  • Uniformity coefficient: ≤1.1

Applications

  • Industrial softening
  • Industrial Demineralization

Recommended Operating Conditions

  • Operating Temperature (Max.): 130℃
  • PH Range: 0-14
  • Min. Bed depth: 800 mm
  • Operation linear velocity: 5-60 m/h (max.)
  • Backwash linear velocity: Approx. 10-25 m/h (at 20°C)
  • Bed expansion: Approx. 4-5 vol.% (at 20°C, per m/h)
  • Backwash Freeboard: 60-100 vol.%

Regeneration Conditions (Counter-current)

RegenerantHClH₂SO₄
Regeneration level (Approx.)50 g/l80 g/l
Concentration (Approx. wt. %)4-6%1-3%
Regeneration linear velocity5 m/h (Approx.)5 m/h (Approx.)
Rinse linear velocity5 m/h (Approx.)5 m/h (Approx.)
Rinse water requirement (slow/fast)2-5 BV2-5 BV

Regeneration Conditions (Co-current)

RegenerantHClH₂SO₄
Regeneration level (Approx.)100 g/l150 g/l
Concentration (Approx. wt. %)6-10%1-3%
Regeneration linear velocity5 m/h (Approx.)5 m/h (Approx.)
Rinse linear velocity5 m/h (Approx.)5 m/h (Approx.)
Rinse water requirement (slow/fast)4-8 BV4-8 BV

Hydraulic Characteristics

Typical values of pressure drop and bed expansion are shown in figures within the original document. Caution should be taken to avoid bed loss due to over-expansion.

Precautions

  • Store in sealed containers or bags above 0°C in dry conditions, away from direct sunlight.
  • Avoid mixing with strong oxidizing agents.
  • In case of eye contact, rinse thoroughly with water and consult a specialist.
  • Dispose of materials according to local regulations.
  • Dry polymers will expand and may generate exothermic reactions when wetted.
  • Spilled materials can be slippery.

Disclaimer This extraction may miss figures, footnotes, or revisions. Contractual data must match the OEM PDF revision used on the project.

Official datasheet (PDF)

Lenntech datasheet mirror

Curated from selected public technical reference material for discovery and preliminary comparison. This summary is not a substitute for a current certified manufacturer datasheet. Verify revisions and design limits before use.