Thermax Tulsion T 52 Na BC UPS
PDF datasheet mirror for Thermax Tulsion T 52 Na BC UPS (Thermax). Verify with OEM before design.
Summary
Product identification
- Product Name: TULSION® T-52 Na BC N
- Product Description: PREMIUM STRONG ACID CATION NUCLEAR GRADE RESIN
- Resin Type: Gel type, produced as moist spherical beads, containing Sulphonic acid as the functional group.
- Features: Excellent resistance to oxidizing agents with high operating capacity. Most suitable for water treatment and suited for use in a wide pH range and elevated temperature conditions. NSF grade resin, conditioned to achieve low VOCs.
Typical Characteristics
- Type: Strong acid cation exchange resin
- Matrix structure: Crosslinked copolymer
- Functional group: Sulphonic
- Physical form: Black colored moist beads
- Ionic form: Sodium
- Screen size USS (wet): 16 to 50
- Particle size (min. 95%): 0.3 to 1.2 mm
- Total exchange capacity (min.): 2.2 meq / ml
- Moisture %: 43 ± 3%
- Backwash settled density: 830 to 860 g/lit
- Temperature stability (max): 140 °C
- pH range: 0 to 14
- Solubility: Insoluble in all common solvents.
Typical Operating Conditions
- Maximum operating temperature: 140°C (in Na form)
- Resin bed depth (min): 600 mm
- Maximum service flow: 120 m³/hr/m³
- Backwash expansion space: 40 to 75%
- Backwash flow: 9 to 20 m³/hr/m³
- Regenerant: HCl/ H₂SO₄ for H form; NaCl for Na form
- Regeneration level: 30 to 160 g HCl/l ; 40 to 250g/l H₂SO₄ ; 60 to 160 NaCl g/l
- Regenerant concentration: 3 to 4% HCl; 1.5 to 5% H₂SO₄; 10 to 15% NaCl
- Regenerant flow rate: 2 to 16 m³/hr/m³
- Regeneration time: 20 to 60 min.
- Rinse flow rate (Slow): At regeneration flow rate
- Rinse flow rate (Fast): At service flow rate
- Rinse Volume: 3 to 5 m³/m³
Testing
Sampling and testing are performed as per standard testing procedures: ASTMD-2187 and IS-7330, 1998.
Packing
- Super Sack: 1000 lit (35 cft)
- MS drums: 180 lit.
- Fiber Drums: 7 cft
- HDPE lined Bags: 25 lit. (1 cft)
Disclaimer: This data extraction may miss figures, footnotes, or revisions. Contractual data must match the OEM PDF revision used on the project.
Preconditioning of Resin:
- Load resin in the column and backwash with process water to expand the resin bed by at least 50%-60% for 10 minutes. Allow resin to settle and drain water from the column up to the resin bed level.
- Fill the resin column with 2 BV of deionized water and soak for a minimum of 12 hours.
- Drain water up to the resin bed level.
- Carry out brine regeneration using 8 lbs/cft NaCl as a 6% solution at a 2 BV/hr flow rate. Rinse with demineralized water until the effluent is chloride-free.