Back to OLTREMARE
OLTREMARE logo

Datasheet summary

LOW3-4014

Engineering summary from PDF text extraction for LOW3-4014. Verify every value with the OEM datasheet.

Summary

Product identification

  • Model: LOW3-4014
  • Type: Low Energy, Excellent Productivity - Brackish Water Element
  • Configuration: Spiral Wound
  • Membrane Polymer: Composite Polyamide
  • Brine Spacer Material: Polypropylene

Product water

  • Permeate Flow: 620 gpd (2.35 m³/d)
  • Nominal Salt Rejection: 98.5%
  • Minimum Salt Rejection: 97.0%
  • Nominal Membrane Area: 19 ft² (1.8 m²)

Test Conditions:

  • NaCl Solution: 1500 ppm
  • Applied Pressure: 150 psi (10.3 bar)
  • Operating Temperature: 77 °F (25 °C)
  • Permeate Recovery: 10%
  • Permeate pH (after 30 min): 6.5 – 7.0

Operating limits

  • Maximum Operating Pressure:
    • Fiberglassed: 600 psi (41.4 bar)
    • Tape Wrapped: 300 psi (20.7 bar)
  • Maximum Temperature: 113 °F (45 °C)
  • Maximum Pressure Drop: 10 psi (0.7 bar)
  • Maximum Feed Flow: 12 gpm (45.4 lpm)
  • Maximum Chlorine Concentration: <0.1 ppm

Feed water

  • Feedwater pH Range: 3.0 – 10.0
  • Maximum Feedwater SDI (15min): 5.0
  • Maximum Feedwater Turbidity: 1.0 NTU
  • Minimum ratio of concentrate to permeate flow for any element: 5:1

Mechanical / hydraulic

  • Dimensions:
    • Total Length (A): 14.0 inches (355.6 mm)
    • Diameter (B): 3.95 inches (100.3 mm)
    • Connection Diameter (C): 0.75 inches (19.1 mm)
    • Core Tube Extension Feed Side (DF): 1.2 inches (30.5 mm)
    • Core Tube Extension Concentrate Side (DC): 1.2 inches (30.5 mm)
  • Weight: 3 lbs (1.4 kg)

Additional Information

  • Minimum permeate flow for individual elements: 15 percent below listed flow.
  • Elements are vacuum sealed in a polyethylene bag containing less than 1.0% sodium meta-bisulfite and 10% propylene glycol solution.
  • Permeate obtained from the first hour of operation should be discarded.
  • Avoid static permeate-side backpressure at all times.
  • For element loading, use only glycerine to lubricate o-rings and brine seal.
  • The presence of free chlorine and other oxidizing agents will cause membrane failure; this damage is not covered under warranty.

Disclaimer: This summary is based on extracted text and may omit figures, footnotes, or the latest revisions. Contractual data must match the OEM PDF revision used on the project.